王成,李先芬,刘昊,等.激光熔覆Co1.5CrFeNi1.5Ti0.75Nbx高熵合金的组织和性能研究[J].精密成形工程,2021,13(2):81-86.
WANG Cheng,LI Xian-fen,LIU Hao,et al.Microstructure and Properties of Laser Cladding Co1.5CrFeNi1.5Ti0.75Nbx High-Entropy Alloy[J].Journal of Netshape Forming Engineering,2021,13(2):81-86.
激光熔覆Co1.5CrFeNi1.5Ti0.75Nbx高熵合金的组织和性能研究
Microstructure and Properties of Laser Cladding Co1.5CrFeNi1.5Ti0.75Nbx High-Entropy Alloy
投稿时间:2020-12-04  
DOI:10.3969/j.issn.1674-6457.2021.02.013
中文关键词: 高熵合金  Laves相  X射线衍射  耐磨性
英文关键词: high entropy alloy  Laves phase  X-Ray diffraction  wear resistance
基金项目:合肥工业大学2020年国家级大学生创新创业训练计划(202010359013)
作者单位
王成 合肥工业大学 材料科学与工程学院合肥 230009 
李先芬 合肥工业大学 材料科学与工程学院合肥 230009 
刘昊 合肥工业大学 材料科学与工程学院合肥 230009 
陈路林 合肥工业大学 材料科学与工程学院合肥 230009 
刘强 合肥工业大学 材料科学与工程学院合肥 230009 
曹岳 合肥工业大学 材料科学与工程学院合肥 230009 
陈森 合肥工业大学 材料科学与工程学院合肥 230009 
摘要点击次数: 2448
全文下载次数: 1118
中文摘要:
      目的 研究Nb含量对高熵合金Co1.5CrFeNi1.5Ti0.75Nbx熔覆层组织和性能的影响。方法 在H13钢表面制备了Co1.5CrFeNi1.5Ti0.75Nbx(x=0.25,0.50,0.75,1.00,原子数分数)高熵合金熔覆层,研究Nb含量对熔覆层的物相组织、微观结构、硬度和耐磨性的影响。结果 高熵合金熔覆层主要为BCC相、FCC相和Laves相的组织。在熔覆层中添加Nb,Laves相随之增加,组织的微观形貌发生变化。熔覆层的硬度远远高于H13钢(退火态),Co1.5CrFeNi1.5Ti0.75Nb0.5熔覆层的平均硬度最高,约为H13钢(退火态)的2.8倍。Co1.5CrFeNi1.5Ti0.75Nb0.5熔覆层的摩擦磨损失重最小,磨损程度更低,耐磨性更好。结论 Nb元素加入高熵合金体系会形成Laves相,Laves相能够提高高熵合金的力学性能。相关结果对于高熵合金体系的研究具有一定意义,为高熵合金的成分设计和优化提供了必要的实验支持。
英文摘要:
      The work aims to study the effect of Nb content on the structure and properties of the high-entropy alloy Co1.5CrFeNi1.5Ti0.75Nbx cladding layer. The Co1.5CrFeNi1.5Ti0.75Nbx (x=0.25, 0.50, 0.75, 1.00) high-entropy alloy cladding layer was prepared on the surface of H13 steel, and the influence of Nb content on the phase structure, microstructure, hardness and abrasive resistance of the cladding layer was studied. The high-entropy alloy cladding layer was mainly composed of BCC phase, FCC phase and Laves phase. When Nb was added to the cladding layer, the Laves phase increased, and the microstructure of the structure changed. The hardness of the cladding layer was much higher than that of H13 steel (annealed), and the average hardness of the Co1.5CrFeNi1.5Ti0.75Nb0.5 cladding layer was the highest, which was about 2.8 times that of H13 steel (annealed). The Co1.5CrFeNi1.5Ti0.75Nb0.5 cladding layer had the smallest friction and wear loss, lower wear degree and better wear resistance. The addition of Nb element to the high-entropy alloy system will form the Laves phase, which can improve the mechanical properties of the high-entropy alloy. The relevant results have certain significance for the study of high-entropy alloy systems, and provide necessary experimental support for the composition design and optimization of high-entropy alloys.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第12072916位访问者    渝ICP备15012534号-6

>版权所有:《精密成形工程》编辑部 2014 All Rights Reserved

>邮编:400039 电话:023-68679125传真:02368792396 Email: jmcxgc@163.com

>    

渝公网安备 50010702501719号