文章摘要
余耀晖,王成,程旋,等.Al/Cu双金属管内旋压增量成形有限元数值模拟与分析[J].精密成形工程,2018,10(4):41-47.
YU Yao-hui,WANG Cheng,CHENG Xuan,et al.Finite Element Numerical Simulation and Analysis of Incremental Forming of Al/Cu Double Metal Tube Inner Spinning[J].Journal of Netshape Forming Engineering,2018,10(4):41-47.
Al/Cu双金属管内旋压增量成形有限元数值模拟与分析
Finite Element Numerical Simulation and Analysis of Incremental Forming of Al/Cu Double Metal Tube Inner Spinning
投稿时间:2018-06-09  修订日期:2018-07-10
DOI:10.3969/j.issn.1674-6457.2018.04.006
中文关键词: 双金属复合管  内旋压成形  数值模拟  成形质量
英文关键词: double metal composite pipe  internal spinning forming  numerical simulation  forming quality
基金项目:航空科学基金(2016ZE52047);江苏省自然科学基金(BK20151469);江苏高校优势学科建设工程
作者单位
余耀晖 1. 南京航空航天大学 材料科学与技术学院南京 2100162. 江苏省核能装备材料工程实验室南京 210016 
王成 1. 南京航空航天大学 材料科学与技术学院南京 2100162. 江苏省核能装备材料工程实验室南京 210016 
程旋 1. 南京航空航天大学 材料科学与技术学院南京 2100162. 江苏省核能装备材料工程实验室南京 210016 
魏文斌 1. 南京航空航天大学 材料科学与技术学院南京 2100162. 江苏省核能装备材料工程实验室南京 210016 
熊昊 1. 南京航空航天大学 材料科学与技术学院南京 2100162. 江苏省核能装备材料工程实验室南京 210016 
陶杰 1. 南京航空航天大学 材料科学与技术学院南京 2100162. 江苏省核能装备材料工程实验室南京 210016 
摘要点击次数: 3690
全文下载次数: 2945
中文摘要:
      目的 分析Al/Cu双金属管在内旋压增量成形时应力、应变、剪切结合强度的分布情况,研究主要工艺参数对双金属管剪切结合强度的影响规律。方法 基于有限元模拟软件,对Al/Cu双金属管内旋压成形过程进行有限元数值模拟;研究了内旋压增量成形时工艺参数:内管减薄率ψ、两管之间的初始间隙c、旋轮进给比f对剪切结合强度的影响。结果 随着工艺参数内管减薄率ψ、两管之间的初始间隙c、旋轮进给比f的增大,剪切应力数值也随着增大;基管与衬管的高剪切应力值主要集中在旋压结束部分,衬管的长度被拉长,模拟与实验的剪切应力在旋压成形的末端数值明显增大。结论通过有限元数值模拟分析,得出不同的工艺参数对成形质量的影响规律,对实际成形有重要的作用。
英文摘要:
      The paper aims to study distribution of stress, strain, shear bond strength and influences of main process parameters of Al/Cu bimetallic tube on the shear bonding strength of bimetallic tub. Based on finite element simulation software, finite element numerical simulation of the spinning process of Al/Cu bimetallic tube was carried out. Influences of process parameters (the reduction rate of the inner tube ψ, the initial gap c between the two tubes, roller feed ratios f) on shear and bonding strength in the inner spinning incremental forming were studied:. With the increase of process parameters of the tube thinning rateψ, the initial gap c between the two tubes, roller feed ratios f, the shear stress value also increased. The high shear stress values of the base pipe and the liner were mainly concentrated at the end of the spinning. The length of the liner was elongated, and the simulated and experimental shear stress increased significantly at the end of spin forming. Through the finite element numerical simulation and analysis, the influences of different process parameters on the forming quality are obtained, which plays an important role in the actual production.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第12242886位访问者    渝ICP备15012534号-6

>版权所有:《精密成形工程》编辑部 2014 All Rights Reserved

>邮编:400039 电话:023-68679125传真:02368792396 Email: jmcxgc@163.com

>    

渝公网安备 50010702501719号