文章摘要
林艳丽,何祝斌,姚坤伟.铝合金薄壁管热态内压成形的变形控制[J].精密成形工程,2015,7(1):36-41.
LIN Yan-li,HE Zhu-bin,YAO Kun-wei.On the Deformation Control during IHPF of Thin-walled Aluminum Alloy Tube at Elevated Temperature[J].Journal of Netshape Forming Engineering,2015,7(1):36-41.
铝合金薄壁管热态内压成形的变形控制
On the Deformation Control during IHPF of Thin-walled Aluminum Alloy Tube at Elevated Temperature
投稿时间:2014-12-16  修订日期:2015-01-10
DOI:10.3969/j.issn.1674-6457.2015.01.007
中文关键词: 内高压成形  铝合金管  热态气压成形  变形  成形性能
英文关键词: internal high pressure forming (IHPF)  aluminum alloy tube  hot metal gas forming (HMGF)  deformation  formability
基金项目:国家自然科学基金资助项目(51405102);教育部新世纪优秀人才支持计划( NCET-11-0799);教育部创新团队子课题(IDGA18102063)
作者单位
林艳丽 哈尔滨工业大学(威海), 山东威海264209 
何祝斌 哈尔滨工业大学, 哈尔滨150001 
姚坤伟 哈尔滨工业大学, 哈尔滨150001 
摘要点击次数: 3822
全文下载次数: 3476
中文摘要:
      薄壁管材热态内压成形时,管材内部各处受到均匀内压的作用,但是由于管材各处的温度和边界条件不同,所以将产生复杂的变形过程。讨论热态内压成形时影响管材变形的主要因素,揭示管材热态内压成形时产生不均匀变形的主要原因。在此基础上,结合实例说明如何从控制温度分布和模具约束条件2 个方面来控制管材的变形。采用不均匀温度分布,可改变各区域材料的变形抗力和摩擦状况,提高管材零件的壁厚均匀性;采用局部快速加热,可实现长管状零件的局部成形而无需大尺寸的模具;采用局部模具约束,可改变不同区域变形的先后顺序、有效控制变形的不均匀性,从而提高管材的成形性能。
英文摘要:
      The inner of the thin-walled tube is subjected uniform internal pressure during hot pressure forming. Because of the difference of temperature and boundary conditions for different part of the tube, the tube will undergo complex deformation process. The paper discussed the main factors affecting the tube deformation in hot pressure forming, and the main reasons for the uneven deformation have been obtained. On this basis, how to control the tube deformation through controlling temperature distribution and die constraint was illustrated by way of example. The use of non-uniform temperature distribution can alter the regional deformation resistance and friction conditions, also improve the uniformity of the tube thickness. The use of local rapid heating can achieve the local forming of long tubular parts without large dies. The use of local die constrains can change the order of the deformation in different areas and control the non-uniformity of deformation effectively, therefore can improve the forming performance of the tube.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第12325859位访问者    渝ICP备15012534号-6

>版权所有:《精密成形工程》编辑部 2014 All Rights Reserved

>邮编:400039 电话:023-68679125传真:02368792396 Email: jmcxgc@163.com

>    

渝公网安备 50010702501719号